Capability
Cold heading
Forms the head and body from wire without cutting, so the grain follows the shape instead of being severed.
Best once the volume justifies the tooling. We will tell you where that threshold falls for your part.
What we have written about it

Brass Cold Heading Economics
Cold heading saves material and cycle time, so it should be cheaper. On large-diameter brass at moderate annual volumes it frequently is not, and the arithmetic is easy…

Cold Heading Upset Ratio Cold Shut
One blow upsets about 2.25 wire diameters, two blows about 4.5. Past that, the wire folds into a cold shut.

Cold Heading Defects Shoulder Screw
Dents, flaking, flash, under-filled shoulders and thread defects on a cold-headed shoulder screw: real photos, the tool that causes each one, and what to write in your…
Cold Heading vs CNC Machining Custom Fasteners
Cold heading can produce a lower unit cost than CNC machining, especially at higher volumes. But a lower piece price does not automatically mean a lower project cost.
Parts of this kind
These are parts we have produced. Which process a given part goes through depends on its geometry and quantity — send the part and we will tell you which one yours needs.